Resulting Anodized Aluminum surface flooding after staining were the following main reasons:
1 piece caustic pre-treatment is not thorough enough.
(2) low melt temperature dyeing.
3 staining solution surface oil.
4 film did not retire net rework.
5 oxide film is contaminated.
6 After oxidation washed thoroughly enough, not cleaned.
7 aluminum anodizing current density is too large.
8 anodizing solution temperature is too low, the current density is too small.
9 aluminum anodizing solution temperature.